advantages

Laminated magnet

  • (schematic diagram of magnetic Field)

  • (laminated magnet’s Layers)

  • (Schematic diagram of eddy current)

  • (Schematic diagram of thermal simulation)

  • Insulation thickness: 70-100 um
  • Insulation layers: 2-40 layers
  • Max working temp. of the magnet: 60-250 ℃
  • Temp. resistance of the magnet surface coating: -60-300℃
  • Corrosion resistance of the magnet surface coating: Neutral salt spray resistance can be over 500 hrs and PCT can be over 200 hrs